Main products and kinetics of the thermal degradation of polyamids.
Chemosphere 42, 601-607 (2001)
The thermal degradation of the polyamides (PA) 6, 12, 66 and 612 was investigated by means of thermal analysis/mass spectrometry (TA-MS) and pyrolysis in a german standard oven. Sample masses were about 20 and 40 mg. The heating rates used in the dynamic studies were 1, 5 and 10 K min(-1). Both air and nitrogen atmospheres were utilized. The kinetic parameters were calculated from the TA-MS measurements and the main decomposition products were registered online. The evolved products from the pyrolysis oven were captured and analyzed off-line by GC/MS.
Impact Factor
Scopus SNIP
Scopus
Cited By
Cited By
Altmetric
1.033
0.000
53
Annotations
Special Publikation
Hide on homepage
Publication type
Article: Journal article
Document type
Scientific Article
Keywords
Thermal decomposition; Pyrolysis; Dynamic measurements; TA-MS
Language
english
Publication Year
2001
HGF-reported in Year
0
ISSN (print) / ISBN
0045-6535
e-ISSN
1879-1298
Journal
Chemosphere
Quellenangaben
Volume: 42 ,
Issue: 5,
Pages: 601-607
Publisher
Elsevier
Publishing Place
Kidlington, Oxford
Reviewing status
Peer reviewed
Institute(s)
Institute of Ecological Chemistry (IOEC)
PSP Element(s)
G-505100-003
Scopus ID
0035125298
PubMed ID
11219685
Erfassungsdatum
2001-12-31